Alloy Steel

Engineering alloy steels for shafts, gears, couplings, tooling and heavy machined components. Supplied in the as-rolled, annealed or quenched and tempered condition with full mill certification.

14 grades stocked6 forms availableFull mill certification

[ 01 ] Grades in this family

Alloy Steel

Showing 14 of 14

AISI 4140 / 42CrMo4

AISI 4140 / 42CrMo4

Ex-stock Dubai
AISI 4140EN 42CrMo4 / 1.7225

The benchmark chromium-molybdenum through-hardening engineering steel. Excellent combination of strength, toughness and machinability in the quenched and tempered condition.

3 forms available
AISI 4340 / 34CrNiMo6

AISI 4340 / 34CrNiMo6

Mill indent
AISI 4340EN 34CrNiMo6 / 1.6582

Nickel-chromium-molybdenum steel with very high hardenability and toughness in heavy sections, chosen for the most highly stressed machined components.

2 forms available
SA387 Grade 11 Class 2

SA387 Grade 11 Class 2

Mill indent
ASTM / ASME A387 / SA387 Grade 11 Class 2EN 13CrMoSi5-5 / 1.7336

1.25Cr-0.5Mo-Si pressure vessel plate. The silicon addition improves oxidation resistance, making Grade 11 the common choice for hot wall vessels and hydrogen service up to around 550 C where full 2.25Cr strength is not required.

3 forms available
SA387 Grade 12 Class 2

SA387 Grade 12 Class 2

Mill indent
ASTM / ASME A387 / SA387 Grade 12 Class 2EN 13CrMo4-5 / 1.7335

1Cr-0.5Mo pressure vessel plate. The economical Cr-Mo grade for moderate temperature pressure parts, widely used for separator and drum shells where creep and hydrogen resistance are needed but the duty is below the 2.25Cr range.

3 forms available
SA387 Grade 22 Class 2

SA387 Grade 22 Class 2

Mill indent
ASTM / ASME A387 / SA387 Grade 22 Class 2EN 10CrMo9-10 / 1.7380

2.25Cr-1Mo pressure vessel plate — the refinery standard for hydroprocessing. The higher chromium and molybdenum push the Nelson curve limit well above Grade 11, which is why reactors, separators and hot wall equipment in hydrogen service specify it.

3 forms available
SA387 Grade 5 Class 2

SA387 Grade 5 Class 2

Mill indent
ASTM / ASME A387 / SA387 Grade 5 Class 2EN X12CrMo5 / 1.7362

5Cr-0.5Mo plate. The chromium level lifts resistance to sulphidic corrosion and high temperature oxidation, so Grade 5 is specified for crude and vacuum unit hot sections where naphthenic and sulphur attack dominate.

3 forms available
SA387 Grade 9 Class 2

SA387 Grade 9 Class 2

Mill indent
ASTM / ASME A387 / SA387 Grade 9 Class 2EN X11CrMo9-1 / 1.7386

9Cr-1Mo plate for high temperature service. Used where sulphidic corrosion resistance and creep strength have to be carried above the 5Cr range, typically in refinery heaters and transfer line equipment.

3 forms available
SA387 Grade 91 Class 2

SA387 Grade 91 Class 2

Mill indent
ASTM / ASME A387 / SA387 Grade 91 Class 2EN X10CrMoVNb9-1 / 1.4903

Modified 9Cr-1Mo-V (Grade 91) plate. Vanadium and niobium micro-alloying gives roughly twice the creep rupture strength of Grade 22 at 550 - 600 C, enabling thinner, lighter pressure parts in supercritical steam and high temperature process plant. Heat treatment and PWHT control are critical and are recorded on the certificate.

3 forms available
A335 P11 Seamless Pipe

A335 P11 Seamless Pipe

Mill indent
ASTM / ASME A335 / SA335 Grade P11EN 13CrMoSi5-5 / 1.7336

1.25Cr-0.5Mo seamless pipe. The matching pipe grade to SA387 Grade 11, used for moderate temperature steam and process lines where plain carbon steel loses strength and oxidation resistance.

3 forms available
A335 P12 Seamless Pipe

A335 P12 Seamless Pipe

Mill indent
ASTM / ASME A335 / SA335 Grade P12EN 13CrMo4-5 / 1.7335

1Cr-0.5Mo seamless pipe. The economical Cr-Mo pipe grade for boiler feed, steam and hot process service up to around 540 C, and the usual partner to SA387 Grade 12 plate.

3 forms available
A335 P22 Seamless Pipe

A335 P22 Seamless Pipe

Mill indent
ASTM / ASME A335 / SA335 Grade P22EN 10CrMo9-10 / 1.7380

2.25Cr-1Mo seamless pipe — the main steam and hot reheat standard. P22 carries creep strength and hydrogen resistance across refinery hot wall piping, superheater headers and heater coils, and is the pipe most often paired with SA387 Grade 22 vessels.

3 forms available
A335 P5 Seamless Pipe

A335 P5 Seamless Pipe

Mill indent
ASTM / ASME A335 / SA335 Grade P5EN X12CrMo5 / 1.7362

5Cr-0.5Mo seamless pipe for sulphidic and naphthenic service. Specified on crude and vacuum transfer lines and heater passes where sulphur attack, not pressure, sets the material.

3 forms available
A335 P9 Seamless Pipe

A335 P9 Seamless Pipe

Mill indent
ASTM / ASME A335 / SA335 Grade P9EN X11CrMo9-1 / 1.7386

9Cr-1Mo seamless pipe. Higher chromium for oxidation and sulphidic corrosion resistance in refinery heater coils and high temperature transfer lines.

3 forms available
A335 P91 Seamless Pipe

A335 P91 Seamless Pipe

Mill indent
ASTM / ASME A335 / SA335 Grade P91EN X10CrMoVNb9-1 / 1.4903

Modified 9Cr-1Mo-V (P91) seamless pipe for supercritical steam. The creep strength allows a much thinner wall than P22 at 580 - 600 C, cutting weight and thermal fatigue on main steam and hot reheat lines. Hardness after PWHT is reported on every length.

3 forms available

Need a grade or size not listed?

Our Dubai desk sources direct from the mills. Send your requirement and we will revert with availability.