A335 P22 Seamless Pipe

ASTM / ASME A335 / SA335 Grade P22EN 10CrMo9-10 / 1.7380Fittings / flanges A234 WP22 / A182 F22
Stock statusMill indent
Typical lead time4 - 8 weeks mill indent

2.25Cr-1Mo seamless pipe — the main steam and hot reheat standard. P22 carries creep strength and hydrogen resistance across refinery hot wall piping, superheater headers and heater coils, and is the pipe most often paired with SA387 Grade 22 vessels.

  • Seamless, normalised and tempered to ASME SA335
  • Creep rupture strength for long term elevated temperature service
  • Matched fittings (A234 WP) and flanges (A182 F) available from one source
  • Hardness, hydro and ultrasonic test reports with every heat

Available forms & sizes

FormSize range
Seamless Pipes & Tubes1/2" - 24" NB, SCH 40 - SCH 160 / XXS
Fittings1/2" - 24" butt weld fittings, WP11 / WP22 / WP91
Flanges1/2" - 24", 150# - 2500#, F11 / F12 / F22 / F5 / F9 / F91

Chemical composition (%)

ElementMinMax
C0.050.15
Cr2.002.50
Mo0.901.10
Si-0.50
Mn0.300.60

Mechanical properties

PropertyValueUnit
Yield Strength (0.2%)205 minMPa
Tensile Strength415 minMPa
Elongation20 min (longitudinal)%
ConditionNormalised and tempered, seamless-

Physical properties

PropertyValueUnit
Density7.85g/cm3
Max Service Temperature550 - 650 depending on gradeC

Typical applications

Main steam and hot reheat piping
Superheater and reheater headers
Refinery hot wall piping and heater coils
High temperature process lines

Frequently asked

[ 02 ] Other grades in Alloy Steel

AISI 4140 / 42CrMo4

AISI 4140 / 42CrMo4

Ex-stock Dubai
AISI 4140EN 42CrMo4 / 1.7225

The benchmark chromium-molybdenum through-hardening engineering steel. Excellent combination of strength, toughness and machinability in the quenched and tempered condition.

3 forms available
AISI 4340 / 34CrNiMo6

AISI 4340 / 34CrNiMo6

Mill indent
AISI 4340EN 34CrNiMo6 / 1.6582

Nickel-chromium-molybdenum steel with very high hardenability and toughness in heavy sections, chosen for the most highly stressed machined components.

2 forms available
SA387 Grade 11 Class 2

SA387 Grade 11 Class 2

Mill indent
ASTM / ASME A387 / SA387 Grade 11 Class 2EN 13CrMoSi5-5 / 1.7336

1.25Cr-0.5Mo-Si pressure vessel plate. The silicon addition improves oxidation resistance, making Grade 11 the common choice for hot wall vessels and hydrogen service up to around 550 C where full 2.25Cr strength is not required.

3 forms available
SA387 Grade 12 Class 2

SA387 Grade 12 Class 2

Mill indent
ASTM / ASME A387 / SA387 Grade 12 Class 2EN 13CrMo4-5 / 1.7335

1Cr-0.5Mo pressure vessel plate. The economical Cr-Mo grade for moderate temperature pressure parts, widely used for separator and drum shells where creep and hydrogen resistance are needed but the duty is below the 2.25Cr range.

3 forms available
SA387 Grade 22 Class 2

SA387 Grade 22 Class 2

Mill indent
ASTM / ASME A387 / SA387 Grade 22 Class 2EN 10CrMo9-10 / 1.7380

2.25Cr-1Mo pressure vessel plate — the refinery standard for hydroprocessing. The higher chromium and molybdenum push the Nelson curve limit well above Grade 11, which is why reactors, separators and hot wall equipment in hydrogen service specify it.

3 forms available
SA387 Grade 5 Class 2

SA387 Grade 5 Class 2

Mill indent
ASTM / ASME A387 / SA387 Grade 5 Class 2EN X12CrMo5 / 1.7362

5Cr-0.5Mo plate. The chromium level lifts resistance to sulphidic corrosion and high temperature oxidation, so Grade 5 is specified for crude and vacuum unit hot sections where naphthenic and sulphur attack dominate.

3 forms available
Download DatasheetAR