[ 01 ]
Alloy Steel
A335 P11 Seamless Pipe
Mill indent1.25Cr-0.5Mo seamless pipe. The matching pipe grade to SA387 Grade 11, used for moderate temperature steam and process lines where plain carbon steel loses strength and oxidation resistance.
A335 P12 Seamless Pipe
Mill indent1Cr-0.5Mo seamless pipe. The economical Cr-Mo pipe grade for boiler feed, steam and hot process service up to around 540 C, and the usual partner to SA387 Grade 12 plate.
A335 P22 Seamless Pipe
Mill indent2.25Cr-1Mo seamless pipe — the main steam and hot reheat standard. P22 carries creep strength and hydrogen resistance across refinery hot wall piping, superheater headers and heater coils, and is the pipe most often paired with SA387 Grade 22 vessels.
A335 P5 Seamless Pipe
Mill indent5Cr-0.5Mo seamless pipe for sulphidic and naphthenic service. Specified on crude and vacuum transfer lines and heater passes where sulphur attack, not pressure, sets the material.
A335 P9 Seamless Pipe
Mill indent9Cr-1Mo seamless pipe. Higher chromium for oxidation and sulphidic corrosion resistance in refinery heater coils and high temperature transfer lines.
A335 P91 Seamless Pipe
Mill indentModified 9Cr-1Mo-V (P91) seamless pipe for supercritical steam. The creep strength allows a much thinner wall than P22 at 580 - 600 C, cutting weight and thermal fatigue on main steam and hot reheat lines. Hardness after PWHT is reported on every length.
[ 02 ]
Cupro Nickel
Cupro Nickel 90/10 Seamless Pipes
Mill indentThe default seawater alloy. 90% copper with 10% nickel and a controlled iron addition builds a protective cuprous oxide film in seawater, and the inherent copper toxicity stops macrofouling — barnacles and mussels do not settle, so cooling lines stay clean without chlorination. Specified for ship and platform seawater systems, firewater ring mains and condenser tubing where the velocity stays below about 3.5 m/s.
Cupro Nickel 70/30 Seamless Pipes
Mill indentThe higher-duty cupro nickel. Tripling the nickel to 30% raises strength, erosion-corrosion resistance and the allowable seawater velocity to around 4.5 m/s, and lifts the service temperature well above 90/10. It is the grade for pump and valve-adjacent piping, hot brine and MSF desalination heat recovery, and any line where turbulence or sand loading would strip the film off 90/10.
Cupro Nickel 66/30/2/2 (C71640)
Project supplyThe desalination variant of 70/30. Raising iron and manganese to about 2% each stabilises the protective film under high velocity, sand-laden and partly deaerated brine, which is exactly the duty inside MSF evaporator heat recovery and reject sections. Where 70/30 tubes thin at the inlet ends, C71640 holds.
[ 03 ]
Duplex & Super Duplex
Duplex 2205
Ex-stock DubaiThe most widely used duplex grade. Roughly double the yield strength of 316L, allowing thinner and lighter sections while delivering far better chloride stress corrosion cracking resistance.
Super Duplex 2507
Mill indentSuper duplex with PREN above 40 for the most aggressive seawater and sour service. S32760 (Zeron 100) adds tungsten and copper for enhanced acid resistance.
[ 04 ]
Nickel Alloys
Inconel 625
Mill indentNickel-chromium-molybdenum alloy strengthened by niobium. Exceptional strength and corrosion resistance from cryogenic temperatures to 980 C without heat treatment.
Inconel 600
Mill indentSolid solution nickel-chromium-iron alloy with high resistance to oxidation, carburisation and chloride ion stress corrosion cracking at elevated temperature.
Monel 400
Mill indentNickel-copper alloy with outstanding resistance to flowing seawater, hydrofluoric acid and alkalis, and total immunity to chloride stress corrosion cracking.
Hastelloy C276
Mill indentNickel-molybdenum-chromium alloy with tungsten, regarded as the most universally corrosion resistant alloy available for both oxidising and reducing media.
Alloy 800 (Incoloy 800)
Mill indentIron-nickel-chromium alloy for high temperature strength with oxidation and carburisation resistance. The 32Ni-21Cr balance resists chloride stress corrosion cracking that austenitic stainless suffers, which is why it is standard for process heater and reformer tubing.
Alloy 800HT (Incoloy 800HT)
Mill indentThe creep-optimised version of Alloy 800. Controlled carbon plus a combined aluminium and titanium window of 0.85 - 1.20% gives far better creep rupture strength above 600 C, so 800HT is the grade for the hottest reformer and pigtail service rather than plain 800.
Alloy 825 (Incoloy 825)
Mill indentNickel-iron-chromium with molybdenum, copper and titanium. The combination handles both reducing and oxidising acids and resists chloride stress corrosion cracking and sour well fluids, making 825 the standard CRA for sour service tubulars, cladding and acid plant.
Alloy 617
Mill indentNickel-chromium-cobalt-molybdenum alloy for the extreme end of high temperature service. Solid solution strengthening keeps useful creep strength to 1100 C while the chromium and aluminium give oxidation resistance, so 617 is used where 800HT and stainless are long past their limit.
Alloy 740H
Project supplyPrecipitation-hardened nickel alloy developed for advanced ultra-supercritical boilers. Gamma-prime strengthening plus about 25% chromium holds creep rupture strength and coal-ash corrosion resistance at 750 C and above, which is beyond what 617 can carry in thick section steam headers.
[ 05 ]
OCTG & Line Pipe
API 5L X52 / L360
Mill indentThe baseline transmission grade. X52 balances weldability against pressure rating, which is why it remains the default for gathering lines, utility piping and plant interconnects where wall thickness rather than yield strength drives the design.
API 5L X65 / L450
Mill indentThe workhorse offshore and high-pressure grade. The higher yield allows a thinner wall at the same design pressure, cutting pipe weight on risers and long tie-backs, and X65 is the grade most often specified with sour service and HIC testing.
API 5L X70 / L485
Mill indentHigh strength thermomechanically rolled line pipe for long distance, large diameter transmission. X70 is specified where the pipeline economics are driven by wall thickness and steel tonnage over hundreds of kilometres.
[ 06 ]
Stainless Steel
304 / 304L
Ex-stock DubaiThe workhorse austenitic stainless steel. 304L's lower carbon content prevents carbide precipitation during welding, making it the default choice for welded fabrications that cannot be post-weld annealed.
316 / 316L
Ex-stock DubaiMolybdenum-bearing austenitic stainless steel. The 2-3% Mo addition transforms pitting resistance in chloride-bearing media, making 316L the baseline grade for marine and chemical service in the Gulf.
321 / 347
Ex-stock DubaiTitanium and niobium stabilised austenitic grades. The stabilising addition ties up carbon so the steel resists intergranular corrosion after prolonged exposure in the 425-815 C sensitisation range.
904L
Mill indentHigh alloy austenitic grade with 4-5% molybdenum and copper, bridging the gap between 316L and nickel alloys for sulphuric and phosphoric acid service.
310S Stainless Steel
Mill indentThe high-temperature austenitic. 25Cr-20Ni gives scaling resistance to around 1035 C in continuous service, so 310S is the grade for furnace internals, radiant tubes and anything that lives in flue gas rather than in water.
317L Stainless Steel
Mill indentA molybdenum-up step on 316L. Raising Mo to 3 - 4% lifts PREN to around 30, which buys real margin against pitting and crevice attack in pulp, scrubber and chloride service where 316L is borderline but duplex is more than the duty needs.
316Ti Stainless Steel
Mill indentTitanium-stabilised 316. The titanium ties up carbon so the steel keeps its intergranular corrosion resistance after long exposure in the 425 - 815 C sensitisation range, and it holds higher creep strength than 316L in hot service.