904L

UNS N08904EN 1.4539
Stock statusMill indent
Typical lead time4 - 8 weeks mill indent

High alloy austenitic grade with 4-5% molybdenum and copper, bridging the gap between 316L and nickel alloys for sulphuric and phosphoric acid service.

  • Resists reducing and oxidising acids
  • Copper-enhanced acid resistance

Available forms & sizes

FormSize range
Plates1.5 - 100 mm thk, up to 2500 mm wide
Seamless Pipes & Tubes1/2" - 24" NB, SCH 5S - SCH 160
Round Bars6 - 500 mm dia
Flanges1/2" - 48", 150# - 2500#
Fittings1/2" - 48", SCH 10S - SCH 160

Chemical composition (%)

ElementMinMax
C-0.020
Cr19.023.0
Ni23.028.0
Mo4.05.0
Cu1.02.0

Mechanical properties

PropertyValueUnit
Yield Strength (0.2%)220 minMPa
Tensile Strength490 minMPa
Elongation35 min%

Physical properties

PropertyValueUnit
Density8.0g/cm3
PREN36-

Typical applications

Sulphuric acid plant equipment
Flue gas scrubbers
Seawater handling
Phosphoric acid service

Frequently asked

[ 02 ] Other grades in Stainless Steel

304 / 304L

304 / 304L

Ex-stock Dubai
UNS S30400 / S30403EN 1.4301 / 1.4307

The workhorse austenitic stainless steel. 304L's lower carbon content prevents carbide precipitation during welding, making it the default choice for welded fabrications that cannot be post-weld annealed.

6 forms available
316 / 316L

316 / 316L

Ex-stock Dubai
UNS S31600 / S31603EN 1.4401 / 1.4404

Molybdenum-bearing austenitic stainless steel. The 2-3% Mo addition transforms pitting resistance in chloride-bearing media, making 316L the baseline grade for marine and chemical service in the Gulf.

6 forms available
321 / 347

321 / 347

Ex-stock Dubai
UNS S32100 / S34700EN 1.4541 / 1.4550

Titanium and niobium stabilised austenitic grades. The stabilising addition ties up carbon so the steel resists intergranular corrosion after prolonged exposure in the 425-815 C sensitisation range.

5 forms available
310S Stainless Steel

310S Stainless Steel

Mill indent
UNS S31008EN 1.4845 / X8CrNi25-21

The high-temperature austenitic. 25Cr-20Ni gives scaling resistance to around 1035 C in continuous service, so 310S is the grade for furnace internals, radiant tubes and anything that lives in flue gas rather than in water.

6 forms available
317L Stainless Steel

317L Stainless Steel

Mill indent
UNS S31703EN 1.4438 / X2CrNiMo18-15-4

A molybdenum-up step on 316L. Raising Mo to 3 - 4% lifts PREN to around 30, which buys real margin against pitting and crevice attack in pulp, scrubber and chloride service where 316L is borderline but duplex is more than the duty needs.

6 forms available
316Ti Stainless Steel

316Ti Stainless Steel

Mill indent
UNS S31635EN 1.4571 / X6CrNiMoTi17-12-2

Titanium-stabilised 316. The titanium ties up carbon so the steel keeps its intergranular corrosion resistance after long exposure in the 425 - 815 C sensitisation range, and it holds higher creep strength than 316L in hot service.

6 forms available
Download DatasheetAR